Corrosions Can be Avoid By The Way Of Helical Dead End

2021/11/04 15:27

1. Get rid of the dirt at the surface of the helical useless quit , after which uniformly coat a floor of the electrical strength fitting with a coating for growing the toughness and flexibility of the suitable;


2. Coating a layer of epoxy resin on the proper, and laying a layer of glass fabric before the epoxy resin is solidified;


3. Apply two layers of epoxy resin at the floor of the glass material with the glass fabric. after the 2 layers of epoxy resin are solidified, apply 3 layers of epoxy resin and lay  layers of glass cloth earlier than the 3 layers of epoxy resin are solidified. 4 layers of epoxy had been then carried out to the 2 layers of glass material. one or more layers of epoxy resin are persisted to be implemented over the fourth layer of epoxy. one or greater layers of epoxy resin are continued to be applied over the second one layer of epoxy. the anti-corrosion fittings consist of: a flexible layer layer-by means of-layer covered at the steel fitting, a covered epoxy layer, a layer of glass cloth laid, and a coated two-layer epoxy resin. a three-layer epoxy resin layered on a two-layer epoxy resin, a -layer glass fabric laid, and a four-layer epoxy resin coated. the anti-corrosion strength fittings synthetic by means of the new approach have the blessings of corrosion resistance, desirable insulation performance, excellent mechanical load bearing, flexibility and sturdiness.

Helical Dead End.png